主要成份% |
C碳 |
Si矽 |
Mn锰 |
Cr(铬) |
W(钨) |
P(磷) |
S(硫) |
0.93-1.00 |
/0.15-0.50 |
0.90-1.20 |
0.50-1.00 |
0.50-1.00 |
0.025以下 |
0.010以下 |
Quenching: Pre-heat up to 550-650℃ and again heat up to 800-850℃; then quench in oil; Backfire: Heat up to 150-200℃ and stay in this temperature; then cool in still air; Hardness: more than HRC60℃; Forging: 1050-850℃; Anneal: Heat up to 750-800℃ and stay for 1-3hours in this temperature then cool slowly in furnace; Uses: This steel is not easy to deform after heat treatment, so it is adapted for making precision instrument, precision measuring apparatus, reamer, milling cutter, screw die, screw tap and various punching dies, etc.. Specification: round (MM) 22-28-32-38-45-50-58-65-75-85-95 105-115-130-155-165-185-205-235-260-280-310 Flat (MM) 10X208-258-308-358-410-460-510-610 13X208-258-308-358-410-460-510-610 16X208-258-308-358-410-460-510-610 20X208-258-308-358-410-460-510-610 25X208-258-308-358-410-460-510-610 30X208-258-308-358-410-460-510-610 35X208-258-308-358-410-460-510-610 40X208-258-308-358-410-460-510-610 45X208-258-308-358-410-460-510-610 50X208-258-308-358-410-460-510-610 55X208-258-308-358-410-460-510-610 60X208-258-308-358-410-460-510-610 70X208-258-308-358-410-460-510-610 80X208-258-308-358-410-460-510-610 |